Answers about concrete preparation, coating systems, moisture, cure times and pricing in Ontario. Filter by topic, service or sub-service to find what applies to your floor.
Coatings bond mechanically to a profiled surface. If the slab still carries laitance, oil, an old sealer or a weak top layer, the new coating bonds to that instead of sound concrete, and it can come away with it. Mechanical preparation — diamond grinding or shot blasting — removes those layers and creates the profile the product requires. It's the least visible part of the job and the one that decides whether the floor lasts.
Related: concrete surface preparation and surface preparation and grinding.
A grind-and-seal densifies and seals the existing concrete — good for dust control on a sound slab where appearance and chemical exposure aren't the priority. A full resinous coating builds a film on top, which gives more resistance to spills and abrasion, colour for zoning and line marking, and a surface that's easier to clean. The right answer depends on the slab condition, what's spilled on it, and the traffic it carries.
An industrial building heated to a stable temperature can meet coating requirements through winter. The practical problem is loading docks and overhead doors, which let cold air sweep across the floor. We plan which doors stay closed, measure slab temperature and dew point during installation and cure, and phase areas near doors for times when they can be kept shut.
Related: industrial epoxy flooring and concrete coating services.
Saw-cut and construction joints take an impact every time a forklift crosses. Once an edge chips, the damage accelerates, and the joint becomes a trip point and a source of shock loading for equipment. We cut back damaged edges, rebuild them, and fill with a semi-rigid filler suited to wheel traffic. Coating over broken joints without repairing them usually means the coating fails along the same lines.
Related: joint filling and concrete repair and restoration.
Most Vaughan warehouses can't close, so the installation is planned around the operation. We section the floor into areas that come out of use in turn, agree forklift and foot traffic routes, and schedule the most disruptive stages — grinding and coating — for nights or weekends where needed. Each section is returned once it has reached the cure stated for the traffic it will carry.
Related: industrial epoxy flooring and fast return-to-service flooring.
Odour depends heavily on the chemistry. Some products carry a noticeable smell during application and for a period after; others are formulated to be lower-odour. In an occupied home we look at the product's data for odour and ventilation requirements, plan airflow, and agree timing with you — for example, whether anyone sensitive to odours should be out of the house for part of the day.
Related: solid color epoxy flooring and concrete coating services.
A garage heated to a steady temperature can meet a product's requirements in the middle of winter. What trips it up is the door: opening it lets cold air across a curing floor and can pull the slab temperature down quickly. We confirm the space can hold temperature before booking, check readings on the day, and agree when the door stays shut. Ventilation still has to be managed during application.
Related: polyaspartic garage flooring and flake epoxy flooring.
A basement slab sits in contact with the ground, and moisture can move up through it even when the surface looks dry. A coating sealed over that moisture can trap it, and the pressure can push the coating off as blisters or peeling. Testing — commonly by in-situ relative humidity under ASTM F2170, or by the calcium chloride method under ASTM F1869 — tells us whether the slab is within the limit the chosen product allows. If it isn't, a moisture-mitigating primer can be specified where the manufacturer supports it.
Related: moisture and substrate systems and concrete coating services.
Heated basements are often the best winter work there is, because conditions are stable. What matters is holding the slab and air temperature within the product's range and above the dew point through the whole cure, and managing ventilation while people are living upstairs. We check conditions on the day and test the slab for moisture before we start, because basements carry moisture risks that garages don't.
Related: solid color epoxy flooring and concrete coating services.
Every product's technical data sheet gives a cure time for light foot traffic and a longer one for vehicle traffic, and both lengthen as temperature drops. Polyaspartic topcoats generally return to service faster than conventional epoxy systems, which is one reason they're used in Ontario garages. Hot tires on a floor that hasn't fully cured can mark it, so we give you a specific time for your floor on the day, based on the product and conditions, rather than a general number.
Related: fast-cure flooring systems.
Scaling is loss of the top layer of concrete, usually in patches, and is commonly linked to freeze-thaw exposure with de-icing salts. Cracking is a break through the slab, which can come from shrinkage as the concrete cured, settlement, or movement. Most garage cracks are shrinkage cracks and can be treated before coating. Cracks that are widening, uneven across the break, or accompanied by settlement are a different matter, and a structural engineer should look at those before any coating decision is made.
Related: concrete repair and restoration.
The first few feet inside a garage door take the most punishment in an Ontario winter: snow falls off the car, melts, pools with dissolved salt, and freezes again when the door opens. That zone also has the widest temperature swings. Surface scaling — thin flakes coming away — often starts there, and it can also point to a weaker surface layer from how the slab was originally finished. We assess it before recommending anything, because the fix depends on how deep the damage runs.
Related: concrete crack repair and concrete repair and restoration.